The cut was off and took some square sanding with 220 grit on the sanding block.
The tube had a slight dent that would show up with paint applied.
I filled it with some thinned CWF and followed with 400 grit sanding.
There was some molding flash on the nose cone end plug.
The nose cone tip had some mold lines at the rounded tip.
On the left is the before -
On the right is after sanding with 400 grit.