Thursday, February 19, 2015

TLP Pershing #K046 Build, Part 38, Dang!

I play guitar so I've got fingernails. I try to be careful when sanding but I scratched and scarred a balsa fin pad!

TIP: A water based filler (like CWF) won't stick to the gray primer.
Squadron Putty has solvents (sticks and fills plastic model joints) and was used on the scratches.
While the putty was still wet (it dries quickly) the excess was taken off with a flat blade knife.




Here's the pad after sanding.
The white putty is easy to see against the gray primer filler.